● High absorption coefficient
● Large stimulated emission cross section
● Wide absorption band
● High damage threshold
● Uniaxial crystal
Chemical Formula,Crystal:Activator | YVO4: Nd3+ |
Activator Concentration | Nd3+: 0.1~3.0at% |
Optical Axial Angle | +/-0.5° |
Wavefront Distortion | λ/8 per inch @632.8nm |
Dimensions | As customized |
Tolerance | Diameter:±0.02mm ,Length:±0.2mm |
Parallelism | ≤10″ |
Perpendicularity | ≤5′ |
Surface Flatness | λ/10 per inch @632.8nm |
Surface Quality | 10-5(MIL-PRF-13830B) |
Clear Aperture | >95% |
Damage Threshold | >750MW/cm2 |
Coating | AR、HR as required |
Note: Parameters above can be customized as required. |