● High slope efficiency, operates at room temperature
● Flash lamp pumping or laser diode pumping is both available
Host | Yttrium Aluminium Garnet (Y3Al5O12) |
Dopant Concentration | Cr3+:0.3~1.2at%,Tm3+:5~6at%,Ho3+:0.3~0.4at% |
Growth Direction of Crystal | [111] ,<5° |
Wavefront Distortion | ≤λ/8 per inch@632.8nm |
Extinction Ratio | ≥25dB |
Dimensions | Diameter:3~6mm , Length:50~120mm |
Dimensional Tolerances | Diameter:﹢0.00/-0.05mm, Length±0.5m |
Barrel Surface | Fine ground, Polished or Grooved |
Parallelism | ≤10″ |
Perpendicularity | ≤5′ |
Surface Flatness | λ/10 per inch @632.8nm |
Surface Quality | 10-5(MIL-PRF-13830B) |
Chamfer | 0.15±0.05mm |
AR Coating Reflectivity | R≤0.20%@2094nm |
Note: Parameters above can be customized as required. |